tel
+86-21-6420 0566

summary:
Main Features of Radiator Powder CoatingExcellent leveling properties, with high gloss and high color saturationExceptional adhesionGood delayed impact resistan...
Excellent leveling properties, with high gloss and high color saturation
Exceptional adhesion
Good delayed impact resistance; the coating remains highly flexible even after several years
Capable of meeting post-forming requirements and withstanding repeated bending
Superior oil resistance and cooking oil resistance, allowing for repeated cleaning
Low-temperature curing (120°C for 25 minutes), saving 25% of baking energy and reducing coating costs.
High transfer efficiency and large coverage area; each kilogram of powder can cover 8-9 square meters, saving 30% of raw materials.
| Item | Quality Indicator | Test Method |
|---|---|---|
| Appearance | Uniform color, loose without lumps, dry powder flowability 120-140 mm | Visual inspection |
| Color | As per customer requirements | Combination of colorimeter and visual inspection |
| Adhesion | Cross-cut test (ISO 2409. GB/T 9286-1998) | 0 level, excellent |
| Impact Resistance | Impact tester (drop weight method) (ISO 6272. GB/T 1732-1993) | Good performance at 50 kg.cm |
| Bending | Bending test instrument (ISO 1519. GB 6742-1986) | 3 mm, excellent flexibility |
| Cupping Test | ISO 1520. GB/T 9753-1993 | Pass at 8 mm |
| Surface Hardness | Pencil hardness (Mitsubishi pencil) (ASTM D3363. GB/T 6739-1996) | 1H-2H |
| Salt Spray Test | ISO 7253. GB/T 1771-1991 | Over 1000 hours |
Radiators